TY - JOUR
T1 - Formation and characteristics of coarsening resistant cubic sigma phase in Al-4 center dot 2Cu-1 center dot 6Mg-0 center dot 2Si
JO - MATER SCI TECH SER
PY - 1997/08/01
AU - Barr SC
AU - Rylands LM
AU - Jones H
AU - Rainforth WM
ED -
VL - 13
IS - 8
SP - 655
EP - 659
Y2 - 2025/05/30